Vinyltriethoxysilane is a dual-function organocylile compound, also known by the names Triethoxy(vinyl)silane, Vinyltriethoxysilane, Ethenyltriethoxysilane, and VTES. This product, CAS No 78-08-0, contains a vinyl group at one end that can react with organic polymers, and a triethoxysilyl group at the other end, which carries three ethoxy groups that can be hydrolyzed with water. Thanks to this double reactivity, it can form a chemical bridge between organic polymers and inorganic surfaces such as glass, silica, metal oxide, mineral filler, and ceramics. Vinyltriethoxysilane can therefore be used as a crosslinker, adhesion promoter, binding agent, surface conditioner, filler surface treatment agent, co-monomer, and moisture retainer.
The most important feature of vinyltriethoxysilane is that it can interact with two different chemical media, organic and inorganic, on the same molecule. The vinyl group can react with polyethylene, acrylic systems and other suitable polymers by free radical mechanism. The triethoxysilyl group hydrolyzes in the presence of moisture to form silanol groups. The formed silanol groups can react with hydroxyl groups on glass, silica, metal oxide and mineral surfaces or condense among themselves and form Si-O-Si bonds. Thus, a stronger and more moisture-resistant interface is formed between the polymer and the inorganic phase.
Commercial high-purity Vinyltriethoxysilane is generally a colorless, low-viscosity, and volatile liquid. Its molecular formula is C8H18O3Si, and its molecular weight is approximately 190.31 g/mol. In Evonik's current Dynasylan VTEO technical data, the density is given as approximately 0.91 g/cm3 at 20 °C, the boiling point is approximately 161 °C, the flash point is approximately 46 °C, and the viscosity is approximately 0.7 mPa·s. When the product reacts with water and moisture, the ethoxy groups hydrolyze and ethanol is released. Therefore, moisture control is important in storage, mixing, and surface pretreatment processes.
Although Vinyltriethoxysilane functions similarly to Trimethoxyvinylsilane, it is not the same product. Trimethoxyvinylsilane carries methoxy groups and forms methanol in hydrolysis. Vinyltriethoxysilane carries ethoxy groups and forms ethanol in hydrolysis. The hydrolysis of ethoxy groups is generally slower than that of methoxy groups. Therefore, Vinyltriethoxysilane may provide an advantage in surface treatment systems where more controlled hydrolysis, longer processing time, and lower methanol formation are desired.
WHAT IS VINYLTRIETHOXYSILANE?
Vinyltriethoxysilane is an organofunctional silane in which a vinyl group and three ethoxy groups are attached to the silicon atom. It is also chemically defined as Triethoxy(vinyl)silane or Ethenyltriethoxysilane. The name Vinyltriethoxysilane can be used in Turkish. Its common abbreviation is VTES or VTEO. The molecule has two different chemical functions in the same structure. The first function is the vinyl group. The vinyl group contains a carbon-carbon double bond and can participate in free radical reactions. This group can form chemical bonds with polyethylene, acrylic polymers, and other suitable organic systems. The second function is the triethoxysilyl group. Three ethoxy groups attached to the silicon atom can be hydrolyzed with water. During hydrolysis, ethanol is formed and silanol groups are formed on silicon. These silanol groups can condense with Si-OH, Al-OH or metal-OH groups on inorganic surfaces. As a result, Si-O-Si or Si-O-metal-like bonds can be formed. This dual function distinguishes Vinyltriethoxysilane from the classic solvent or surfactant. The product is essentially a reactive binding agent that regulates the interfacial chemistry. It helps establish a chemical connection between the organic polymer phase and the inorganic filler or surface.
Key functions of vinyltriethoxysilane:
Providing moisture cross-linking in polyethylene
Increasing adhesion between mineral fillers and polymer
Improving coating adhesion on glass and ceramic surfaces
Supporting coating adhesion on metal surfaces
Making the surface of the fillings more hydrophobic
Improving filler-polymer compatibility
Supporting mechanical properties in mineral-filled plastics
Enhancing wet adhesion in polymer dispersions
Consuming trace amounts of water in mastics
To gain vinyl function in organic synthesis
To be used as a binding agent in free radical curing systems
Supporting the production of cross-linked polyethylene in cable insulation and piping applications
Evonik states that Vinyltriethoxysilane can be used in the preparation of moisture-curing polymers such as polyethylene. In the typical process, silane is grafted into the polymer during extrusion with the help of a peroxide initiator. Then, as a result of contact with moisture, silanol groups are formed and polymer chains are cross-linked via siloxane bonds. Another important use of Vinyltriethoxysilane is mineral-filled polymers. Silane is bonded to the filler surface on one side. The vinyl group can be bonded to the polymer matrix. In this way, interfacial strength can be improved. When the filler surface becomes more hydrophobic, it can be better wetted by the polymer. Dispersion may improve. Melting viscosity may decrease. Preservation of mechanical and electrical properties may become easier under moisture.
COMMON PRODUCT AND CHEMICAL NAMES
Vinyltriethoxysilane
Triethoxy(vinyl)silane
Triethoxyvinylsilane
Vinyltriethoxysilane
Ethenyltriethoxysilane
Triethoxyethenylsilane
Silane, ethenyltriethoxy-
VTES
VTEO
Vinyl Silane
CAS NO, EC / EINECS NO AND CHEMICAL IDENTIFICATION
Product Name: Vinyltriethoxysilane
English name: Vinyltriethoxysilane
Common abbreviations: VTES, VTEO
CAS No: 78-08-0
EC/EINECS No: 201-081-7
Molecular formula: C8H18O3Si
Structural notation: CH2=CH-Si(OC2H5)3
Molecular weight: Approximately 190.31 g/mol
Chemical class: Organofunctional alkoxysylan
Organic function: Vinyl group
Hydrolyzable function: Three ethoxy groups
Physical form: Liquid
Appearance: Colorless and clear
Density, 20 °C: Approx. 0.91 g/cm3
Boiling point: About 160-161 °C
Flash point: About 44-46°C
Viscosity, 20 °C: Approx. 0.7 mPa·s
Refractive index: Approximately 1,396
Main function: Silane binding agent
Vinyltriethoxysilane is commercially offered in high purity. The actual purity, water content, color, density and refractive index of the product must be verified from the supplier's current TDS and COA documents. In particular, the amount of water is a critical quality parameter. Moisture can initiate the hydrolysis of the product and cause oligomerization during storage.
CHEMICAL STRUCTURE AND MOLECULAR PROPERTIES OF VINYLTRIETHOXYSILANE
In the vinyltriethoxysilane molecule, the silicon atom makes four bonds. One of these bonds is directly attached to the vinyl group. The other three bonds go to the ethoxy groups.
The structure can be represented simply as: CH2=CH-Si(OC2H5)3
The vinyl group is the center of organic reactivity. The carbon-carbon double bond can be activated by free radical initiators.
Peroxides or suitable radical sources can react the vinyl group with the polymer chain. This mechanism is used in cross-linking polyethylene with silane. The triethoxysilyl group is the center of inorganic reactivity. Ethoxy groups react with water.
This reaction is called hydrolysis.
Simplified: Si-OC2H5 + H2O → Si-OH + C2H5OH.
As a result of the hydrolysis of each ethoxy group, an ethanol molecule can be formed. At the end of complete hydrolysis, three silanol groups can form on silicon. Silanol groups can condense with each other. Water can be separated between the two silanols and a siloxane bond can be formed. Si-OH + HO-Si → Si-O-Si + H2O
Silanol groups can also condense with hydroxyl groups on glass, silica or mineral surfaces. As a result of this reaction, the silane molecule chemically bonds to the surface. This mechanism is the basis of filler and surface treatment. The ethoxy groups of Vinyltriethoxysilane are larger and more hydrophobic than the methoxy groups. This structure reduces the hydrolysis rate. In the Gelest technical data, it is stated that the hydrolysis rate of Vinyltriethoxysilane is significantly lower than that of Vinyltrimethoxysilane. For this reason, VTES can be preferred in surface treatment systems where more controlled hydrolysis is required.
Important properties of the molecule:
Organic group with vinyl function
Three hydrolyzable ethoxy groups
Silicon-carbon bond
Double bond that can participate in free radical reactions
Creating silanol with moisture
Creating ethanol in hydrolysis
Creating a siloxane network with condensation
Chemical bonding to mineral surfaces
Grafting into polymers
Ability to increase surface hydrophobicity
Low viscosity
Controlled hydrolysis behavior
Moisture sensitivity
PHYSICAL AND CHEMICAL PROPERTIES OF VINYLTRIETHOXYSILANE
Vinyltriethoxysilane is a colorless, clear and low viscosity liquid in pure or high purity commercial form. In the Evonik Dynasylan VTEO technical information, the product is described as colorless and low viscosity organosylane.
General technical specifications:
Physical appearance: Colorless clear liquid
Chemical character: Triethoxysilane with vinyl function
Molecular weight: Approximately 190.31 g/mol
Boiling point: About 160-161 °C
Density, 20 °C: Approx. 0.91 g/cm3
Viscosity, 20 °C: Approx. 0.7 mPa·s
Flash point: About 44-46°C
Refractive index: Approximately 1,396
Vapour pressure, 20 °C: Declarable at approx. 5 mmHg
Behavior with water: Hydrolysis occurs
Hydrolysis product: Silanol groups and ethanol
Volatility: Medium
Vinyltriethoxysilane is not only physically soluble in water.
It reacts chemically with water.
Limited miscibility may be seen initially.
Then the ethoxy groups are hydrolyzed.
As hydrolysis proceeds, silanol and oligomeric siloxane species are formed.
For this reason, silane solutions prepared with water should not be stored for a long time.
The rate of hydrolysis depends on the pH.
Acidic and basic conditions can accelerate hydrolysis.
Slightly acidic pH is frequently used in surface treatment solutions.
However, after hydrolysis, the condensation of silanol groups among themselves also begins.
Therefore, the processing time and service life of the pre-hydrolysis solution should be controlled.
Due to its flash point of approximately 44-46 °C, the product should be handled with caution as a flammable liquid.
Ignition sources should be kept away.
Closed system and good ventilation should be preferred.
Ethanol vapor must be considered separately in surface treatment tanks and closed processes, as ethanol is formed during hydrolysis.
HOW DOES VINYLTRIETHOXYSILANE WORK AT THE MOLECULAR LEVEL?
The basic working principle of Vinyltriethoxysilane is based on the molecule reacting with organic and inorganic phases at different ends. The vinyl group can react with the organic polymer. On the other hand, the triethoxysilyl group can form a bond with the inorganic surface after hydrolysis. Therefore, it acts as a molecular bridge. In the case of mineral filler, the process can proceed as follows: Vinyltriethoxysilane reaches the mineral filler surface. In the presence of moisture or controlled water, the ethoxy groups hydrolyze. Silanol groups are formed.
Silanol groups interact with hydroxyl groups present on the mineral surface. As a result of condensation, silane is chemically bonded to the surface. The vinyl part of the molecule is directed outward from the surface.
During polymer processing, the vinyl group can be attached to the polymer matrix by radical mechanism. A stronger interface is formed between the filler and the polymer.
This mechanism is used in composites:
Can increase tensile strength
It can reduce the loss of mechanical properties after moisture
Can improve filler dispersion
It can lower the smelting viscosity
It can facilitate machinability
Reduce the interference of electrical properties by moisture
In the polyethylene cross-linking mechanism, Vinyltriethoxysilane is grafted to the polyethylene chain during extrusion in the presence of peroxide initiator.
The grafted polymer is then brought into contact with moisture.
Ethoxy groups turn into silanol groups.
Silanol groups in neighboring chains condense, forming Si-O-Si bridges.
Polymer chains are cross-linked.
As a result of cross-linking:
Heat resistance
creep resistance
Crack resistance
Chemical Resistance
Abrasion resistance
and shape memory
may develop.
Evonik specifies that silane-crosslinked polyethylene is used especially in low-voltage cable insulation, cable outer sheaths, hot water pipes, plumbing pipes, and underfloor heating systems. Vinyltriethoxysilane can also be used as a co-monomer in polymer dispersions.
It joins the acrylic or styrene-acrylic polymer chain through the vinyl group. During film formation, silane groups can form bonds with inorganic surfaces or among themselves. This mechanism can increase wet adhesion and wet brushing resistance. When using moisture retainers in sealants, the product reacts with trace amounts of water. In this way, premature curing or unwanted reactions caused by water can be reduced.
IN WHICH SECTORS IS VINYLTRIETHOXYSILANE USED?
Vinyltriethoxysilane is used in the polymer, composite, coating, adhesive, cable, and surface treatment industries.
Main areas of use:
Production of cross-linked polyethylene
Cable insulation
Cable outer sheaths
Hot water pipes
Underfloor heating pipes
Plumbing pipes
Mineral-filled thermoplastics
Mineral-filled elastomers
Unsaturated polyester composites
Glass fiber reinforced systems
Silica-filled polymers
Calcium carbonate filled polymers
Alumina and metal oxide-filled systems
Coatings
Paints and primers
Adhesives
Sealants and sealants
Styrene-acrylic dispersions
Acrylic dispersions
Glass surface treatments
Metal surface treatments
Ceramic surface treatments
Pigment and filler surface treatments
Organic synthesis
USES OF VINYLTRIETHOXYSILANE IN POLYETHYLENE CROSSLINKING
One of the most important industrial uses of Vinyltriethoxysilane is the cross-linking of polyethylene by the silane method. Since polyethylene is thermoplastic, it softens at high temperature. Cross-linking creates a chemical network between polymer chains. This network limits chain movement at high temperature.
In the silane crosslinking method, VTES is first grafted to the polyethylene chain. This process can be done with the help of organic peroxide during extrusion. When peroxide is broken down, polymer radicals are formed. These radicals are added to the vinyl group. Silane is attached to the polyethylene chain.
The grafted polyethylene is then cured with moisture. Moisture initiates hydrolysis.
Ethoxy groups transform into silanol groups. Silanol groups condense with appropriate catalyst action. Neighboring polymer chains are linked together by siloxane bonds. Evonik states that the crosslinking step can be carried out under 80-100 °C water bath, steam bath or ambient conditions. The actual curing time depends on the polymer thickness, temperature, moisture amount and catalyst level.
Advantages of cross-linked polyethylene:
Higher heat resistance
Higher creep resistance
Higher crack resistance
Better chemical resistance
Better wear resistance
Better shape memory
USES OF VINYLTRIETHOXYSILANE IN FILLERS AND COMPOSITES
Interfacial incompatibility is a major problem in mineral-filled polymers. Silica, glass and metal oxide surfaces are polar and hydrophilic. Many polymers, such as polyethylene, are more nonpolar. This incompatibility can cause the filler to clump. When vinyltriethoxysilane binds to the mineral surface, the surface becomes more organophilic. The polymer can better wet the filler surface. Dispersion can improve. Aggregation can decrease. Interfacial voids can be reduced Mechanical load can be transferred from the polymer to the filler more efficiently. Evonik technical information states that the silane-treated filler surface becomes more hydrophobic, which can improve filler-polymer compatibility, dispersion and processability. Low melting viscosity is a significant advantage at high filler loads. It is also important to maintain electrical properties after moisture in electrical cable filled compounds. The silane binder can reduce water ingress at the interface.
USES OF VINYLTRIETHOXYSILANE IN COATINGS, ADHESIVES AND SEALANTS
Vinyltriethoxysilane can be used as an adhesion promoter on glass, metal and ceramic surfaces. Hydrolyzed silane forms bonds with hydroxyl groups on the inorganic surface. The vinyl group can bind to the polymer system or be organic overcompatible. This mechanism strengthens the interface between the coating and the surface. It is important to maintain adhesion, especially under moisture. Evonik states that coating glass, metal and ceramic surfaces with VTEO can increase adhesion. When used as a co-monomer in acrylic and styrene-acrylic dispersions, it can be added to the polymer chain through the vinyl group. Wet adhesion and wet brushing resistance may develop in these systems. In mastics, it can be used as a moisture retainer due to its reaction with water. Consuming trace amounts of water can reduce premature curing in moisture-sensitive systems. However, it should not be forgotten that ethanol is formed in this reaction.
IS VINYLTRIETHOXYSILANE USED IN FOOD?
Vinyltriethoxysilane is not a food additive. It should not be added directly to food or beverage. Some silanes can be used in the production of plastics, coatings or composite materials that come into contact with food under certain conditions. This does not mean that Vinyltriethoxysilane is a direct food additive. If it is planned to be used in food contact material, the legislation of the target country, residue in the final material, migration and compliance requirements must be verified separately. Industrial grade Vinyltriethoxysilane should not be added directly to food.
INDUSTRIAL APPLICATIONS OF VINYLTRIETHOXYSILANE
Vinyltriethoxysilane can have multiple functions in different industrial systems. It can be a crosslinker. It can be a binding agent. It can be a surface conditioner. It can be a filler treatment agent. It can be a co-monomer. It can be a moisture retainer. It can be an organic synthesis raw material. It is used in the production of cross-linked polyethylene in the cable industry. It supports the production of polyethylene cross-linked with silane in hot water and underfloor heating pipes in the pipe industry. It forms a bond between mineral fillers and polymer in the composite industry. It can support surface adhesion and moisture control in adhesives and sealants.
In the coating industry, it can increase adhesion to glass, metal, and ceramic surfaces. As a co-monomer in polymer dispersions, it can improve wet adhesion and brushing resistance. It can increase hydrophobicity in filler surface treatments. In organic synthesis, it can be used as an intermediate in the preparation of different functional organosilanes thanks to its reactive vinyl group.
WHAT PROBLEMS CAN VINYLTRIETHOXYSILANE HELP SOLVE?
Poor interfacial adhesion in mineral-filled polymer
Silane can increase interfacial bonding by forming a chemical bridge between the mineral surface and the polymer.
Poor distribution of filler in the polymer
Organophilic nature of the surface can allow the filler to be better wetted by the polymer.
Loss of mechanical properties under moisture
The silane binder can reduce water-induced separation at the interface.
Peeling off the coating from the glass or metal surface
Silane pretreatment can strengthen the bond between the inorganic surface and the coating resin.
High-temperature softening of polyethylene
Crosslinking with silane can improve heat resistance by forming a network between polymer chains.
Creep and deformation of cable insulation
Cross-linked polyethylene can show better shape stability under high temperature.
Unwanted trace moisture in the sealant
Vinyltriethoxysilane can react with water to consume trace moisture.
Poor wet adhesion in styrene-acrylic dispersion
When silane joins the polymer chain as a co-monomer, stronger bonding can form with mineral surfaces.
High smelting viscosity due to filler
Modifying the filler surface with silane can reduce polymer-filler friction.
Very rapid hydrolysis of Trimethoxyvinylsilane
The more slowly hydrolyzed triethoxy structure can widen the process window.
THINGS TO CONSIDER WHEN USING VINYLTRIETHOXYSILANE
Vinyltriethoxysilane reacts with moisture. The package should not be left open for long periods of time. Atmospheric moisture can initiate hydrolysis. Ethanol is formed during hydrolysis. Ethanol vapor can accumulate in closed tanks. Adequate ventilation must be provided. The product has a flash point of about 44-46 °C.
It should be kept away from ignition sources. Static electricity should be checked.
Transfer equipment must be grounded. If pre-hydrolysis is to be performed with water, it must be pH controlled.
Too rapid hydrolysis and condensation may cause precipitation. The pre-hydrolysis solution should not be stored for a long time.
The amount of silane should be optimized according to the surface area. Excessive use of silane does not always result in better adhesion.
A very thick and mechanically weak siloxane layer may form on the surface. Moisture content should be controlled in the filling process. Hydrolysis may be insufficient on a very dry surface. On a very wet surface, silane may condense on its own in solution.
In the polyethylene graft process, the peroxide level should be checked.
Excessive peroxide may cause polymer degradation. TDS should be examined. SDS should be examined. COA should be checked.
INITIAL FORMULATION APPROACHES FOR VINYLTRIETHOXYSILANE
EXAMPLE 1: MOISTURE CROSSLINKABLE POLYETHYLENE STARTER MIX CONTAINING VINYLTRIETHOXYSILANE
Objective: To evaluate the effect of vinyltriethoxysilane level on polyethylene graft yield, crosslinking, temperature resistance and mechanical properties.
Starting composition:
High-density polyethylene: 97.65%
Vinyltriethoxysilane: 1.50%
Dicumyl peroxide: 0.10%
Dibutyltin dilaurate: 0.15%
Irganox 1010: 0.20%
Calcium stearate: 0.40%
Total: 100%
This formulation is a laboratory initial approach.
It is not a commercial cable or pipe recipe.
In actual use, the type of polyethylene, peroxide half-life, extrusion temperature, and target gel amount should be optimized together.
Application approach:
Polyethylene granules are prepared in conditions of low humidity.
Vinyltriethoxysilane, dicumyl peroxide and dibutyltin dilaurate are homogeneously mixed in a separate container.
This liquid mixture is applied on polyethylene granules in a controlled manner.
Irganox 1010 and calcium stearate are added.
The mixture is left to homogenize for a short time in a closed container.
The material is fed into the extruder with the appropriate temperature profile.
Polymer radicals are formed by peroxide breakdown.
Vinyltriethoxysilane is grafted into the polyethylene chain.
The extruded product is cooled.
The samples are cured in an environment of 80-90 °C hot water or high humidity.
The amount of gel is measured at different cure times.
Tensile strength and elongation at break are determined.
Hot pressure or creep test is performed.
The level of vinyltriethoxysilane is comparable to 0.5%, 1.0%, 1.5%, and 2.0%.
Each change is balanced by the amount of polyethylene, maintaining a total of 100%.
EXAMPLE 2: PRE-HYDROLYZED VINYLTRIETHOXYSILANE TREATMENT SOLUTION FOR GLASS AND SILICA SUBSTRATES
Objective: To evaluate the effect of vinyltriethoxysilane level on coating adhesion and wet environment resistance on glass or silica surface.
Starting composition:
Deionized water: 80.0%
Ethanol: 12.0%
Vinyltriethoxysilane: 4.0%
Isopropanol: 3.5%
Acetic acid, 10% aqueous solution: 0.5%
Total: 100%
Application approach:
Deionized water and ethanol are taken into the mixing bowl.
The acetic acid solution is added slowly.
The pH is brought to the range of approximately 4.5-5.0.
Vinyltriethoxysilane is added in a controlled manner in thin stream.
The mixture is hydrolyzed under low-speed stirring for 30-60 minutes.
Isopropanol is added.
It is preferable not to store the prepared solution for a long time.
The glass or silica surface is degreased.
It is rinsed with deionized water.
Silane solution is applied by spraying, dipping or wiping.
Excess solution is removed.
The surface is dried at controlled temperature.
Acrylic or free radical curing coating is applied on top.
Dry adhesion test is performed.
After 24 hours of water immersion, the adhesion test is repeated.
Moisture aging is applied.
The level of vinyltriethoxysilane is comparable to 1%, 2%, 4%, and 6%.
Each change is balanced by the amount of deionized water, maintaining a total of 100%.
SIMILAR PRODUCTS AND ALTERNATIVES TO VINYLTRIETHOXYSILANE
When determining the vinyltriethoxysilane alternative, organic function, hydrolysis group, hydrolysis rate, alcohol formed, polymer type and surface chemistry should be evaluated together.
VINYLTRIETHOXYSILANE AND TRIMETHOXYVINYLSILANE
Both products are vinyl function alkoxysilane.
Vinyltriethoxysilane carries three ethoxy groups.
Trimethoxyvinylsilane carries three methoxy groups.
Trimethoxyvinylsilane generally hydrolyzes more rapidly.
Vinyltriethoxysilane may exhibit slower and controlled hydrolysis.
Trimethoxyvinylsilane forms methanol in hydrolysis.
Vinyltriethoxysilane forms ethanol in hydrolysis.
This difference affects process safety, hydrolysis time, and surface treatment behavior.
Laboratory testing should be performed before substitution directly at the same dose.
VINYLTRIETHOXYSILANE AND METHACRYLOXYPROPYLTRIMETHOXYSILANE
Methacryloxypropyltrimethoxysilane has the function of methacrylate.
Vinyltriethoxysilane directly carries vinyl group.
It blends more directly with methacrylate, silane, acrylic, and methacrylic resins.
Vinyl silane polyethylene can be used more widely in graft process and radical curing systems.
The hydrolysis groups and molecular sizes of the two products are different.
VINYLTRIETHOXYSILANE AND AMINOPROPYLTRIETHOXYSILANE
Aminopropyltriethoxysilane is an amino-function binding agent.
It can show high reactivity in epoxy and isocyanate systems.
Vinyltriethoxysilane carries vinyl function, which can react with free radical mechanism.
In epoxy glue, amino silane may be more suitable.
Vinyl silane is more suitable for polyethylene crosslinking.
VINYLTRIETHOXYSILANE AND GLYCIDOXYPROPYLTRIMETHOXYSILANE
Glycidoxypropyltrimethoxysilane is an epoxy-function organosyllane.
It can react with epoxy and amino resins.
It is a common binding agent in coatings and adhesives.
Vinyltriethoxysilane vinyl is more suitable in systems that work with a radical mechanism due to its function.
QUALITY CONTROL AND PURCHASING CRITERIA FOR VINYLTRIETHOXYSILANE
When purchasing vinyltriethoxysilane, not only the product name and price should be evaluated.
The hydrolysis and graft reactions of silane are sensitive to impurity and water content.
Recommended information to study before buying:
Full product name
Manufacturer
CAS No 78-08-0
EC No 201-081-7
Purity
Gas chromatography analysis result
Outlook
Color
Density
Refractive index
Water content
Free ethanol content
Chloride content
Relevant value if acidity is required
Boiling point
Flash point
Viscosity
Batch number
Country of origin
REACH or KKDIK registration status
TDS
SDS
COA
Packaging type
Shelf life
Moisture-proof packaging integrity
Water content is the critical quality parameter.
High water content can cause premature hydrolysis and oligomerization during storage.
This may alter product reactivity.
Turbidity or increased viscosity can indicate moisture ingress.
When using a new supplier, not only purity but also actual application performance must be compared.
STORAGE AND HANDLING OF VINYLTRIETHOXYSILANE
Vinyltriethoxysilane should be stored protected from moisture. Containers should be kept tightly closed. The product may react with water vapor.
The opened package should be used as soon as possible. A cool and well-ventilated warehouse should be preferred.
It should be kept away from direct sunlight and heat sources. Due to the flash point of about 44-46 °C, flammable liquid storage rules should be applied.
It should be kept away from open flames. Spark sources should be checked. Static electricity accumulation should be prevented.
Transfer equipment must be grounded. Uncontrolled contact with water and strong oxidizers must be avoided. The dehumidified product may hydrolyze. Hydrolysis may result in ethanol and silanol species. Oligomerization may then occur. Evonik reports a shelf life of at least 12 months for Dynasylan VTEO in unopened packaging.
The exact shelf life should be verified from the TDS and packaging label of the commercial product purchased.
VINYLTRIETHOXYSILANE SAFETY INFORMATION
Vinyltriethoxysilane is a flammable organosilane.
Due to its flash point of approximately 44-46 °C, it should be kept away from ignition sources. The accumulation of vapors in the closed environment should be prevented.
Good ventilation should be used. Protective glasses should be used. Chemical resistant gloves should be preferred.
If the risk of splashing is high, face protection can be used. Ethanol is formed during hydrolysis. Ethanol is flammable. For this reason, ventilation is important in closed systems where hydrolysis is carried out with water. In case of contact with eyes, washing with plenty of water should be done. The area in contact with the skin should be cleaned with water.
In the event of a spill, ignition sources should be removed. The product should not be disposed of uncontrollably into drains or surface water.
The exact hazard classification, H statements, P statements, transport class and personal protective equipment must be verified from the current SDS document.
WHAT TO CONSIDER WHEN BUYING VINYLTRIETHOXYSILANE?
In the supply of vinyltriethoxysilane, the application area should be determined first.
Is polyethylene crosslinking?
Is mineral filler surface treatment?
Coating adhesion?
Is sealant moisture control?
Polymer dispersion?
Composite?
This choice influences the required purity and quality parameters.
Information to be clarified before ordering:
CAS No 78-08-0
EC No 201-081-7
Purity level
Water content
Density
Refractive index
Color
Free ethanol
Chloride level
Moisture-proof packaging
Packing quantity
Origin
REACH or KKDIK status
Shelf life
TDS
SDS
COA
If using Trimethoxyvinylsilane as a substitute, the rate of hydrolysis and the alcohol formed must be considered.
Although two products are in the same functional class, they may not exhibit the same process behavior.
Slow hydrolysis may require longer surface treatment time.
In contrast, the processing window of the prepared solution may be wider.
VINYLTRIETHOXYSILANE SUPPLY FROM ATAMAN KIMYA
Vinyltriethoxysilane is a dual-function organosylan used in cross-linked polyethylene, cables, pipes, mineral-filled plastics, composites, coatings, adhesives, sealants, polymer dispersion, and surface treatment applications. The vinyl group at one end can react with organic polymers. The triethoxysilyl group can bind to glass, silica, metal oxide, and other inorganic surfaces by hydrolysis and condensation.
Companies that want to get information about the supply of Vinyltriethoxysilane from Ataman Kimya share their application areas, required purity level, water content limit, packaging preference and technical document needs, facilitating appropriate product evaluation.
CAS No 78-08-0, EC No 201-081-7, purity, density, color, water content, TDS, SDS and COA information should be confirmed before ordering.
Alternatives such as trimethoxyvinylsilane, amino silane, epoxy silane and methacrylate silane can be evaluated separately according to the target polymer and surface.
FREQUENTLY ASKED QUESTIONS ABOUT VINYLTRIETHOXYSILANE
What is Vinyltriethoxysilane?
It is a dual-function organosilane bearing one vinyl group and three hydrolyzable ethoxy groups.
Is triethoxy(vinyl)the same as silane?
Yes.
What is its Turkish name?
Vinyltriethoxysilane.
What is a CAS number?
78-08-0.
What is an EC number?
201-081-7.
What is its molecular formula?
C8H18O3Si.
What is molecular weight?
About 190.31 g/mol.
What is its physical form?
It is a colorless and low viscosity liquid.
What is its density?
At 20 °C, it is about 0.91 g/cm3.
What is boiling point?
It is approximately 160-161 °C.
What is the flash point?
It is about 44-46 °C.
What is its viscosity?
It is about 0.7 mPa·s at 20 °C.
What happens with water?
The ethoxy groups are hydrolyzed and ethanol is formed with silanol groups.
Why is it used as a binding agent?
It can bridge the two phases because the silanol side can bind to the inorganic surface and the vinyl side to the organic polymer.
Is it used in polyethylene?
Yes.
Is it used in the cable industry?
Yes.
Is it used in pipe production?
Yes.
What does it do in mineral-filled plastics?
It can improve dispersion and polymer-filler adhesion by making the filler surface more organophilic.
Is it used in veneers?
Yes.
Why is it used in sealants?
It can act as a moisture retainer by reacting with trace amounts of water.
Is it used in polymer dispersions?
Yes. As a companion monomer, it can improve wet adhesion and brushing resistance.
Is Trimethoxyvinylsilane the same as
Nope.
What is the main difference?
Vinyltriethoxysilane ethoxy carries methoxy groups, while Trimethoxyvinylsilane carries methoxy groups.
Which hydrolyzes faster?
Generally, Trimethoxyvinylsilane hydrolyzes more rapidly.
What does vinyltriethoxysilane form in hydrolysis?
Ethanol.
What does Trimethoxyvinylsilane form in hydrolysis?
Methanol.
Can it be added to food?
It is not a food additive.
Is it flammable?
Yes.
Is it affected by humidity?
Yes. Moisture initiates hydrolysis.
What documents should be requested?
TDS, SDS, and COA are essential documents.
VINYLTRIETHOXYSILANE - TECHNICAL BRIEF
Vinyltriethoxysilane is a dual-function organocylan compound known as Triethoxy(vinyl)silane or Vinyltriethoxysilane. The CAS No is 78-08-0, the EC No is 201-081-7. Its molecular formula is C8H18O3Si and its molecular weight is approximately 190.31 g/mol. The molecule carries one vinyl group and three ethoxy groups.
The vinyl group can participate in free radical reactions with organic polymers. Ethoxy groups are hydrolyzed by moisture. Hydrolysis results in the formation of silanol groups and ethanol. Silanol groups can condense with glass, silica, metal oxide and other hydroxyl inorganic surfaces.
This double reactivity allows it to form a chemical bridge between the organic polymer and the inorganic surface. The commercial product is colorless and low viscosity liquid. Its density is about 0.91 g/cm3. Its boiling point is about 160-161 °C. Its flash point is about 44-46 °C. Its viscosity is about 0.7 mPa·s.
One of the most important uses is the cross-linking of polyethylene with moisture. It can be used in cable insulation, hot water pipes and underfloor heating pipes. It can increase dispersion and polymer-filler adhesion by modifying the filler surface in mineral-filled plastics. It can improve adhesion to glass, metal and ceramic surfaces in coatings. It can increase wet adhesion strength as a co-monomer in acrylic and styrene-acrylic dispersions. It can be used as a moisture retainer in sealants. It may show slower hydrolysis than Trimethoxyvinylsilane. It forms ethanol instead of methanol in hydrolysis. The product should be protected from moisture. Flammable liquid safety measures should be applied. Purity, water content, density, color, refractive index, TDS, SDS and COA should be evaluated together at the time of purchase. It is recommended that companies planning to supply Vinyltriethoxysilane from Ataman Kimya confirm the appropriate commercial product by specifying the application area, target purity, packaging and technical document requirements.